MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Keysor-Century KC1110 Rigid PVC Extrusion Molding Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: A general purpose, low crease-whitening extrusion molding compound. KC1110 has an excellent balance of properties, offering outstanding clarity and gloss, high impact strength, and good color retention. Its excellent dynamic thermal stability enables easy processability with a wide variety of equipment and conditions. This permits extended production runs with minimum maintenance and downtime, and maximum regrind recycling. It is available in clear, with various levels of blue tint as free flowing pellets.

Recommended for user in a wide variety of extrusion applications and profiles where minimum crease whitening is desired.

Property values are typical values. Information provided by Keysor-Century Corporation.

Keysor-Century Corporation is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080ASTM D2240
Tensile Strength, Yield 46.0 MPa6670 psiASTM D638
Modulus of Elasticity 2.22 GPa322 ksiASTM D638
Flexural Yield Strength 81.0 MPa11700 psiASTM D790
Flexural Modulus 2.34 GPa339 ksiASTM D790
Izod Impact, Notched 9.60 J/cm
@Thickness 3.17 mm
18.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Available clear but manufacturer does not quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 1601 Clear 7002 Flexible PVC
Axiall 8150 Rigid PVC, Extrusion & Molding
Colorite Polymers 2007 Rigid PVC
Colorite Polymers 2019F Rigid PVC
Novatec Novablend® 4545 PVC

PKCV09 / 48702

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.