MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

3D Systems LaserForm® Ti Gr5 (A), AFTER STRESS RELIEF Titanium Material
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Titanium alloy fine-tuned for use with ProX DMP 320 metal powder producing technical and medical applications because of its high strength, low density and its excellent biocompatibility. The essential difference between Ti6Al4V ELI (grade 23) and Ti6Al4V (grade 5) is the allowed higher oxygen and iron content in Ti Gr5. This confers improved strength. LaserForm Ti Gr5 (A) is formulated and fine-tuned specifically for 3D Systems DMP 320 metal 3D Printers to deliver highest part quality and best part properties. The print parameter database that 3D Systems provides together with the material has been extensively developed, tested and optimized in 3D Systems’ part production facilities that hold the unique expertise of printing 500,000 challenging production parts year over year. Based on over 1000 test samples the below listed part quality data and mechanical properties give you high planning security. And for a 24/7 production 3D Systems’ thorough Supplier Quality Management System guarantees consistent, monitored material quality for reliable process results.

Material Description: This titanium alloy is commonly used for lightweight and high strength components such as aerospace and motor sports applications. Because of its excellent biocompatibility Ti Gr5 (A) is also very well suited for medical implants, tools and devices and dental prostheses. The essential difference between Ti6Al4V ELI (grade 23) and Ti6Al4V (grade 5) is the allowed higher oxygen and iron content in Ti Gr5. This confers improved strength while slightly reducing ductility. These benefits make LaserForm Ti Gr5 (A) the ideal material for light-weight, high-strength components as required for a broad scope of parts in aerospace, sports and marine products. Its high strength and biocompatibility make it the material of choice for medical tools and devices.

Classification: Parts built with LaserForm Ti Gr5 Alloy have a chemical composition that meets the requirements of ASTM B265, B348 (grade 5), F2924, ISO 5832-3 and Werkstoff Nr. 3.7165.

Information provided by 3D Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.42 g/cc0.160 lb/in³Absolute theoretical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 38 - 4238 - 42
Tensile Strength, Ultimate 1110 - 1210 MPa161000 - 175000 psiVertical direction — Z; ASTM E8M
 1150 - 1210 MPa167000 - 175000 psiHorizontal direction — XY; ASTM E8M
Tensile Strength, Yield 1030 - 1130 MPa149000 - 164000 psiRp0.2%, Vertical direction - Z; ASTM E8M
 1060 - 1120 MPa154000 - 162000 psiRp0.2%, Horizontal direction - XY; ASTM E8M
Elongation at Break 7.0 - 11 %7.0 - 11 %Horizontal direction — XY; ASTM E8M
 7.0 - 11 %7.0 - 11 %Vertical direction — Z; ASTM E8M
Tensile Modulus 10.5 - 12.0 GPa1520 - 1740 ksiYoung's
Charpy Impact >= 20.0 J>= 14.8 ft-lbASTM E23
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.60 µm/m-°C
@Temperature 20.0 - 100 °C
4.78 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 6.70 W/m-K
@Temperature 50.0 °C
46.5 BTU-in/hr-ft²-°F
@Temperature 122 °F
Melting Point 1692 - 1698 °C3078 - 3088 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.75 %5.5 - 6.75 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.050 %<= 0.050 %
Oxygen, O <= 0.20 %<= 0.20 %
Titanium, Ti 87.6 - 91 %87.6 - 91 %Balance
Vanadium, V 3.5 - 4.5 %3.5 - 4.5 %
Yttrium, Y <= 0.0050 %<= 0.0050 %
 
Descriptive Properties
Element<0.1residuals each
 <0.4residuals total
Surface Roughness4-8µmHorizontal direction (XY)
 4-8µmVertical direction (Z)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Titanium Ti-6Al-4V (Grade 5), STA
Titanium Ti-6Al-4V (Grade 5), Annealed Bar
Titanium Ti-6Al-4V (Grade 5), Annealed

PAPPR3176 / 239144

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.