MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Extramet EMT 909 Tungsten Carbide, Medium-Coarse Grade
Categories: Ceramic; Carbide

Material Notes: EMT 909, is a medium grain size grade grade, with a balance of shock resistance/toughness and the wear resistance.

EMT 909 is a homogenous mixture of tungsten carbide grains in a tough cobalt binder matrix. The carbide grains are fused into a solid matrix of cobalt metals. The metal carbide’s grains are “cemented” in the binder metal’s matrix.

Information provided by Extramet

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.4 - 14.6 g/ccISO 3369
Porosity <= 2.0 %A, Basic; ISO 4505
 <= 2.0 %B, Particular; ISO 4505
 <= 2.0 %C-Porosity; ISO 4505
Grain Size <= 1.0 µmAverage
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 1570 - 1630ISO 3878
Modulus of Rupture 3.50 - 3.70 GPaTransverse Rupture Strength
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 8.5 %Metals Basis
Other 1.0 %Other Carbides
Tungsten, W 90.5 %Metals Basis

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EEMT009 / 312240

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.