MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parson Adhesives PARFIX® 3495 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3495 is low viscosity combined with fast cure speed, surface insensitive cyanoacrylate adhesive. It is specifically formulated to bond difficult surfaces with high industrial strength.

Applications:

  • Ideal for bonding rough, porous and acidic surfaces including Wood, Cardboard, Balsa Wood, Rubbers, Plastics, Metals, Leather, etc.
  • Wide variety of industrial manufacturing and repairing applications

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 45 cPLVT Spindle 1 @ 30 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 1450 psiABS; ASTM D1002
 >= 1740 psiPolycarbonate; ASTM D1002
 >= 2610 psiEtched Aluminum; ASTM D1002
 >= 2900 psiGrit Blasted Steel; ASTM D1002
 >= 3190 psiRubbers; ASTM D1002
 2610 - 4060 psi
 >= 3630 psiWood; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D696
Dielectric Constant 2.7ASTM D150
Dielectric Strength 27.0 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 75.0 µm/m-°CASTM D696
Thermal Conductivity 0.100 W/m-KASTM C177
Melting Point 160 - 170 °C
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 122 °CASTM E228
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourFull
 
Descriptive Properties
AppearanceColorless Liquid
Bonding Times<3 secRubbers
 12-18 secCeramics
 1-5 secWood
 2-5 secPlastics
 5-15 secLeather
 8-10 secMetals
CompositionEthyl Cyanoacrylate
Gap Filling0.05 mm
Initial Strength Retained (%)75Gasoline for 1000 hrs at 22°C
 80Gasoline for 500 hrs at 22°C
 85Isopropanol for 500 hrs at 22°C
 85Isopropanol for 1000 hrs at 22°C
 90Motor Oil for 500 hrs at 40°C
 90Motor Oil for 1000 hrs at 40°C
 90Mineral Spirit for 500 hrs at 22°C
 90Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parson Adhesives PARFIX® 3406 Cyanoacrylate Adhesive
Parson Adhesives PARFIX® 3401 Cyanoacrylate Adhesive

PPARSN137 / 186580

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.