MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray TORAYCA™ TLP1060 Nylon 6 + 30% Carbon Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Long carbon fiber reinforced PA6, CF30%, PA6-CF30.

General Torayca™ Notes: TORAYCA™ is a carbon fiber reinforced thermoplastic (CFRTP) that is light weight and features excellent strength, stiffness, dimensional accuracy, and sliding properties. Physical property: Carbon fiber reinforced thermoplastic (CFRTP) offer excellent mechanical strength/rigidity and maintain a combination of characteristics. Lower specific gravity and lightweight, High creep resistance and fatigue resistance, Excellent abrasion resistance and sliding properties. Low molding shrinkage and coefficient of linear expansion, ensuring high dimensional accuracy, Excellent electrical conductivity and electromagnetic shielding performance.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Filler Content 30 %30 %
Water Absorption 2.5 %2.5 %In 23°C water, polymer initially at 50% RH
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/in80x80x3mmt.; Toray Method
Linear Mold Shrinkage, Transverse 0.0020 cm/cm0.0020 in/in80x80x3mmt.; Toray Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 280 MPa
@Temperature 23.0 °C
40600 psi
@Temperature 73.4 °F
ISO 527-1,2
Elongation at Break 2.0 %
@Temperature 23.0 °C
2.0 %
@Temperature 73.4 °F
ISO 527-1,2
Flexural Strength 400 MPa
@Temperature 23.0 °C
58000 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 21.0 GPa
@Temperature 23.0 °C
3050 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
V-Notched; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.010 - 0.10 ohm-cm0.010 - 0.10 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FDSC Method
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1,2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9178 / 248867

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.