MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shandong Dongyue Shenzhou New Material Co Perfluoro-3,6-dioxa-4-methyl-7-octene-sulfonylfluoride (PSVE)
Categories: Other Engineering Material

Material Notes: Conformable with: Q/DYS 010-2007

In normal state, PSVE is a colorless transparent liquid and important monomer of organic fluoride material, and is mainly used to introduce functional sulfonic group into polymer.

Main Applications:

PSVE is one important monomer of perfluorosulfonic ion exchange resin, and it can be copolymerized with TFE to form sulfonic group branched polymer.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc
@Temperature 38.0 °C
0.0614 lb/in³
@Temperature 100 °F
Liquid
Molecular Weight 446 g/mol446 g/mol
Vapor Pressure 0.00200 bar
@Temperature 38.0 °C
1.50 torr
@Temperature 100 °F
Saturated
 
Chemical PropertiesMetricEnglishComments
Critical Temperature 240 °C464 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point 135 °C
@Pressure 0.101 MPa
275 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
CAS16090-14-5
Chemical NamePerfluoro-3,6-dioxa-4-methyl-7-octene-sulfonylfluoride
Molecular FormulaFO2SCF2CF2OCF(CF3)CF2OCFCF2
Purity (%)>97.51st Grade
 >99High Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSHEN004 / 104059

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.