MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Return Polymers RP1410 100% reycle PVC
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: 100% recycled WHITE PVC window pulverized into a 20 mesh powder and blended in large quantities to ensure consistency. Primarily used in fence, window, and siding applications with or without a capstock layer and processed by single and or twin screw extrusion.

Information provided by Return Polymers Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D-792
Bulk Density 0.497 g/cc0.0179 lb/in³ASTM D1895
Particle Mesh Size 20 Mesh20 Mesh3% retention
 120 Mesh120 Mesh97% retention
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 49.45 MPa
@Thickness 3.00 mm
7172 psi
@Thickness 0.118 in
Type I, 2 in/min; ASTM D 1990
Tensile Impact Strength 168 kJ/m²
@Thickness 3.00 mm
80.0 ft-lb/in²
@Thickness 0.118 in
Type S; ASTM D1822
Dart Drop Total Energy 2140 J/cm4.00 ft-lb/mil70 F, 8# wt, ½” conical tup. Maximum value on a 2" strip recorded; ASTM D4226
 
Electrical PropertiesMetricEnglishComments
Hot Wire Ignition, HWI 60 - 119 sec60 - 119 secASTM D3874
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C160 °FASTM D 648-85
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Descriptive Properties
ColorWhite (L > 90)CIELab, D65, 10 degree observer or visual
FormPulverized Powder / Pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRETURN002 / 238936

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.