MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake LF1010AA LLDPE, Butene Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: LF1010AA is a butene LLDPE with excellent mechanical and down gauging advantages. This Kosher compliant product contains zero slip and antiblock, and is suitable for can liners, agricultural film, shrink film, and blending with LDPE. Kosher Compliant. Test specimens for blown film: nominal thickness 1.0 mils fabricated at 2.5:1 BUR. This product has some 21 CFR clearances. Application/Uses: Agricultural films, Trash bags, Shrink films.

Samples tested at 23°C and 50% RH.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³unformulated polymer; ASTM D1505
Thickness 25.4 microns1.00 milBlown Film as Tested
Melt Index of Compound 0.80 g/10 min0.80 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 900 %900 %ASTM D882
Film Elongation at Break, TD 1100 %1100 %ASTM D882
Dart Drop 3.94 g/micron100 g/milASTM D1709
Film Tensile Strength at Break, MD 42.7 MPa6200 psiASTM D882
Film Tensile Strength at Break, TD 27.6 MPa4000 psiASTM D882
1% Secant Modulus, MD 228 MPa33000 psiASTM D882
1% Secant Modulus, TD 269 MPa39000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 221 °C410 - 430 °Fblow melt
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8813 / 222885

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.