MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trinseo Plexiglas® Diffuse™ DR®-66151 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: Plexiglas® Diffuse™ DR®-66151 is a thermoplastic acrylic resin sufficiently concentrated to be used in blend formulations via extrusion to tailor lens properties in the LED lighting market. It has outstanding hiding performance and high impact resistance.

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 - 1.30 g/ccASTM D792
Water Absorption 0.3 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.002 - 0.004 cm/cmASTM D955
Melt Flow 1.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 38ASTM D785
Tensile Strength, Ultimate 5700 psiASTM D638
Elongation at Break 45 %ASTM D638
Tensile Modulus 280000 psiASTM D638
Flexural Strength 8500 psiASTM D790
Flexural Modulus 240000 psiASTM D790
Izod Impact, Notched 0.900 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 216 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 212 °Fannealed; ASTM D648
Vicat Softening Point 212 °F50°C/hr; 50N; ASTM D1525
 224 °F50°C/hr; 10N; ASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Haze >= 100 %
@Thickness 2.03 mm
ASTM D1003
Transmission, Visible 40 %
@Thickness 2.03 mm
ASTM D1003
 
Descriptive Properties
ASTM ClassificationPMMA 0231T0V1ASTM D788

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Plexiglas® Diffuse™ V045-68207 Acrylic Resin
Trinseo Plexiglas® DR® Acrylic
Trinseo Plexiglas® Frosted DR-66080® Acrylic
Overview of materials for Acrylic, Cast
Röhm Acrylite Plus® zdf Impact Acrylic Polymer

PARKG043i / 191489

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.