MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D1161 J (SIS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in the grade nomenclature:
D1161 JSP - supplied as dusted dense pellets
D1161 JS - supplied as dusted crumb
D1161 JU - supplied as undusted crumb

Region: Japan

Uses: Kraton D1161 J Polymer is used in formulating adhesives, sealants and coatings. It is also used as a modifier of bitumen and polymers and in formulating compounds.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/cc
Volatiles <= 1.0 %
@Temperature 110 °C,
Time 7200 sec
<= 1.0 %
@Temperature 230 °F,
Time 2.00 hour
Viscosity 900 - 1700 cP900 - 1700 cP25% Toluene Solution at 25°C; KM 06
Melt Flow 1.3 - 3.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.3 - 3.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Ash <= 1.0 %<= 1.0 %JU; ISO 247
 <= 1.0 %<= 1.0 %JSP; ISO 247
 <= 2.5 %<= 2.5 %JS; ISO 247
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 37
@Time 30.0 sec
37
@Time 0.00833 hour
ISO 7619
Tensile Strength 28.0 MPa4060 psiISO 37
Elongation at Break 1300 %1300 %ISO 37
300% Modulus 0.900 MPa
@Strain 300 %
131 psi
@Strain 300 %
ISO 37
 
Descriptive Properties
ContentBound Styrene15 percent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® D2122 DO (SBS) Compound
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer

PKRA9866 / 132765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.