System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Dow 4012 Low Density Polyethylene (LDPE)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
Material Notes:
Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.918
g/cc
0.0332
lb/in³
ASTM D792
Water Vapor Transmission
27.9
g/m²/day
1.80
g/100 in²/day
at 1 atm; 1.0 mil coating onto 50 lb Kraft paper; ASTM F1249
Thickness
>=
7.62
microns
>=
0.300
mil
Coating Thickness; Extrusion Coating Processability; Dow Method
Melt Index of Compound
12
g/10 min
12
g/10 min
ASTM D1238
Neck In
4.80
cm
1.89
in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Coating Weight
>=
6.40
g/m²
>=
4.00
lb/ream
Extrusion Coating Processability; Dow Method
Mechanical Properties
Metric
English
Comments
Coefficient of Friction, Dynamic
0.60
0.60
(film/film); 1.0 mil coating onto 50 lb Kraft paper; ASTM D1894
Heat Seal Strength Initiation Temperature
105
°C
221
°F
1 lb/in heat seal strength; 1.0 mil coating onto 50 lb Kraft paper; Dow Method
Thermal Properties
Metric
English
Comments
Melting Point
107
°C
225
°F
Dow Method (DSC)
Vicat Softening Point
89.0
°C
192
°F
ASTM D1525
Processing Properties
Metric
English
Comments
Melt Temperature
315
-
327
°C
599
-
621
°F
Extrusion Coating Processability
Descriptive Properties
Line Speed fpm, max
1610
Dow Method
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
Dow 4010 Low Density Polyethylene (LDPE)
Dow 611A Low Density Polyethylene (LDPE)
Dow 620I Linear Low Density Polyethylene (LDPE)
Dow 662I Low Density Polyethylene Resin
PDOW1225 / 30443
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.