MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo STYRON™ 414 HIPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Availability: Latin America; North America

Features: Food Contact Acceptable; High Flow; High Impact Resistance; High Toughness

Uses: Masterbatch

Agency Ratings: FDA 21 CFR 177.1640

UL File Number: E326906

Processing Method: Injection Molding

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inISO 294-4
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
13 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8989ASTM D785
Tensile Strength at Break 16.0 MPa2320 psiASTM D638
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Tensile Modulus 1.50 GPa218 ksiASTM D638
Flexural Strength 24.0 MPa3480 psiASTM D790
Flexural Modulus 1.42 GPa206 ksiASTM D790
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/inCompression Molded; ASTM D256
 1.17 J/cm2.20 ft-lb/inInjection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 82.8 °C181 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FUnannealed; ASTM D648
Vicat Softening Point 96.1 °C205 °FASTM D1525
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 95.6 - 105 °C204 - 221 °FZone 6
Rear Barrel Temperature 218 - 249 °C424 - 480 °F
Middle Barrel Temperature 218 - 249 °C424 - 480 °F
Front Barrel Temperature 199 - 213 °C390 - 415 °F
Nozzle Temperature 213 - 243 °C415 - 469 °F
Zone 1 177 - 193 °C351 - 379 °F
Zone 2 182 - 204 °C360 - 399 °F
Zone 3 188 - 210 °C370 - 410 °F
Zone 4 199 - 216 °C390 - 421 °F
Zone 5 204 - 221 °C399 - 430 °F
Adapter Temperature 193 - 232 °C379 - 450 °F
Die Temperature 199 - 232 °C390 - 450 °F
Melt Temperature 193 - 232 °C379 - 450 °FExtrusion
Mold Temperature 15.6 - 65.6 °C60.0 - 150 °F
Back Pressure 0.200 - 1.20 MPa29.0 - 174 psi
Cushion 0.635 cm0.250 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRINSE1543 / 312236

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.