Notes: Monprene CP-37225 is a high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-37225 is a high density, low hardness, filled, lubricated, RoHS compliant grade suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Filled; General Purpose; High Density; High Specific Gravity; Low Flow; Low Hardness; Lubricated Uses: Consumer Applications; Gaskets; Handles; General Purpose; Tubing RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |