MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Elantas Conap FR-2000 / FR-200 Conapoxy® Resin / Conacure® Hardener
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes:
Epoxy Potting and Encapsulating Systems for Electronic Applications
High technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive and related industries.

Cytec (Conap) FR-2000 / FR-200 Conapoxy® Resin / Conacure® Hardener
A filled system with superior acid resistance. Curing at room temperature or low elevated temperatures.
  • Mix Ratio, Resin/Hardener (by weight): 100/26
Cure Type: Elevated Temperature

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 300 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 3.60e+15 ohm-cm
Dielectric Constant 4.07
@Frequency 1000 Hz
Dielectric Strength 616 V/mil
Dissipation Factor 0.12
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 47.0 °C
Pot Life 40.0 min
@Temperature 25.0 °C
100 grams

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® VCL Carbon Cloth Laminate with Mil R-9299 Resin
Solvay DAPCO™ 3050 Epoxy Potting Compound
Solvay CYCOM® 934 Epoxy-Carbon Fiber PlainWeave Laminate
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy
Elantas Conap FR-1610 / EA-039 Conapoxy® Resin / Conacure® Hardener

PCYTEC56 / 29288

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.