MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chase Electronic Coatings HumiSeal® 1A33NS Urethane Conformal Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: HumiSeal® 1A33NS conformal coating is: urethane chemistry, toluene free, chemically resistant, single component, contains no free isocyanates, RoHS Directive 2011/65/EC compliant, Recognized under UL File Number E105698. HumiSeal 1A33NS conformal coating has: excellent moisture and environmental protection for printed circuit assemblies, fluorescence under UV light for ease of inspection.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D1475
Solids Content 44 %44 %± 2. By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 521 g/l521 g/l
Viscosity 160 - 200 cP160 - 200 cPFed-Std-141, Meth. 4287
Thickness 25.0 - 75.0 microns0.984 - 2.95 milRecommended coating
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 0.0272 GPa3.95 ksiDMA
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.60e+10 ohm1.60e+10 ohmMoisture; MIL-I-46058C
 2.00e+14 ohm2.00e+14 ohmMIL-I-46058C
Dielectric Constant 3.6
@Frequency 1e+6 Hz,
Temperature 25.0 °C
3.6
@Frequency 1e+6 Hz,
Temperature 77.0 °F
ASTM D150-98
Dielectric Breakdown 7500 V7500 VASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.030
@Frequency 1e+6 Hz,
Temperature 77.0 °F
ASTM D150-98
 
Thermal PropertiesMetricEnglishComments
CTE, linear 193 µm/m-°C107 µin/in-°FTMA
Glass Transition Temp, Tg 26.0 °C78.8 °FDSC
 
Processing PropertiesMetricEnglishComments
Cure Time  20.0 min
@Temperature 88.0 °C
0.333 hour
@Temperature 190 °F
Option
 30.0 min
@Temperature 76.0 °C
0.500 hour
@Temperature 169 °F
Option
 43200 min
@Temperature 23.0 °C
720 hour
@Temperature 73.4 °F
Option
Shelf Life 24.0 Month
@Temperature 23.0 °C
24.0 Month
@Temperature 73.4 °F
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C
Fungus ResistancePassesASTM G21
Thermal Shock-65 to 125°Cper MIL_I_46058C, 50 cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS914 / 239775

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.