MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2000 HC FR A Polyester Alloy; Flame Retardant - UV Stabilized - Medical Cleaner Resistant
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: RTP 2000 HC series are polyester alloys designed to withstand the aggressive cleaners used to disinfect medical equipment

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 240 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 464 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 37.9 MPa5500 psiASTM D 638
Elongation at Break >= 50 %>= 50 %ASTM D 638
Tensile Modulus 1.31 GPa190 ksiASTM D 638
Flexural Strength 58.6 MPa8500 psiASTM D 790
Flexural Modulus 1.45 GPa210 ksiASTM D 790
Izod Impact, Notched 6.41 J/cm
@Thickness 3.20 mm
12.0 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C205 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FASTM D 648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 65.6 - 82.2 °C150 - 180 °F
Drying Temperature 87.8 °C
@Time 14400 - 21600 sec
190 °F
@Time 4.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 103 - 138 MPa15000 - 20000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tritan™ MX711 Medical Grade Copolyester
Eastman Tritan™ MX731 Medical Grade Copolyester
Lucite International Lucite® 4F Acrylic Bead Resin
LGC-4-C Precious dental alloy

PQZRA29841 / 206037

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.