MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Levasil WT110 Colloidal silica
Categories: Other Engineering Material

Material Notes: Levasil WT110 is an alkaline, aqueous dispersion of colloidal silica that is approximately 7% solids by weight. The silica dispersion is sodium stabilized and the amorphous silica particles carry a highly negative surface charge. The silica particles are structured to enhance the activity of the dispersion. The particles have also been surface modified with aluminum. The physical appearance of the dispersion is a clear liquid, slightly more viscous than water. Levasil WT110 is produced for world-wide distribution.

CAS number: 7631-86-9

Applications: Levasil WT110 is a specialty product used primarily in water treatment applications to supply charge to assist in flocculation.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
pH 8.58.5
Specific Surface Area 1100 m²/g1100 m²/g
Viscosity 20 cP20 cP
Storage Temperature 5.00 - 35.0 °C41.0 - 95.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Content0.55 wt%Al2O3
 6.5 wt%Silica

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY678 / 286201

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.