MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cabot FCX™ 80 Carbon Support
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Corrosion resistant carbon for fuel cell applications
FCX 80 carbon support is highly graphitic conductive carbon that can deliver superior conductivity and durability when used as a fuel cell catalyst support. FCX 80 carbon can be used also as part of the fuel cell gas diffusion microporous layer. Incorporating FCX 80 carbon support into fuel cell components can:
  • Increase durability of fuel cell catalysts
  • Enable superior stability of fuel cell performance
  • Deliver high fuel cell life cycle at reduced precious metal loading
  • Minimize gas diffusion limitations due to changes in the carbon surface properties
Key applications
  • Fuel cell catalysts
  • Gas diffusion layers (GDLs)
  • Hydrogen fuel cells
  • Flow batteries
CAS number: 1333-86-4

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Surface Area 70 - 90 m²/g70 - 90 m²/gBET nitrogen
 
Descriptive Properties
Content<20 ppmIron
 <20 ppmTotal Co, Cr, Cu, Mn, Ni
OAN120 – 180 ml/100gASTM D2414

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT148 / 315883

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.