CS 7928* is used for reinforcement of a wide range of polyamide grades. High strand integrity; High strand integrity, Excellent free-flowing properties; Suitable for bulk transport and pneumatic conveyance and High mechanical strength in a wide range of polyamide grades Information provided by Lanxess. |