MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC NORYL™ Resin IGN320 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ IGN320 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits high heat resistance, high modulus, very low moisture absorption, and good dimensional stability. NORYL IGN320 resin is an excellent candidate for automotive applications such as ignition coils where heat and high modulus is required.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 12.8 g/10 min
@Load 5.00 kg,
Temperature 300 °C
12.8 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 108 MPa15700 psi5 mm/min; ASTM D638
Tensile Strength, Yield 108 MPa15700 psi5 mm/min; ASTM D638
Elongation at Break 2.4 %2.4 %5 mm/min; ASTM D638
Tensile Modulus 6.26 GPa908 ksi5 mm/min; ASTM D638
Flexural Strength 170 MPa24700 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.72 GPa830 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 101 J74.5 ft-lbASTM D256
Izod Impact, Unnotched 5.12 J/cm9.59 ft-lb/inASTM D4812
Dart Drop, Total Energy 16.0 J11.8 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 33.9 kV/mm
@Thickness 1.60 mm
861 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
@Thickness 3.20 mm
327 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
@Thickness 3.20 mm
316 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 175 °C347 °FRate B/50; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82343 / 290290

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.