MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Schweitzer-Mauduit Argotecâ„¢ 18214 Thermoplastic polyurethane, aromatic polyether
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Thermoplastic polyurethane, aromatic polyether.

Applications: Textile lamination; bladders. Blown film extrusion. Attribute: Smooth surface, soft ether, mid-range softening temperature, USP-certified polymer and FDA CFR 177.1680; 177.2600.

Information provided by Schweitzer-Mauduit International, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 - 254 microns1.00 - 10.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D-2240
Tensile Strength 27.6 MPa4000 psiASTM D-412
Elongation at Break 700 %700 %ASTM D-412
100% Modulus 4.76 MPa690 psiASTM D-412
300% Modulus 6.89 MPa1000 psiASTM D-412
Tear Strength 64.9 kN/m370 pliDie C; D-624
Tensile Set 15 %15 %@ 200% E; ASTM D-412
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
LengthUp to 1000 non-spliced yards
WidthUp to 86"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCHWE905 / 287665

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.