MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 78 Soft Solder Gel Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Flux exerts powerful scavenging action.
  • Non-fuming and water-soluble.
  • Exhibits excellent capillary action.
Description: Superior No. 78 is a non-fuming, water-soluble paste flux formulated for difficult-to-solder metals. The activators include zinc chloride, ammonium chloride, and hydrochloric acid. The flux exerts powerful scavenging action removing the oxide coatings and other impurities from most metals yielding strong joints. Due to its high viscosity, the flux does not migrate upon heating helping the solder stay in place.

Applications: Superior No. 78 is excellent for use on stainless steel, monel, high chrome alloys, inconel, nickel, copper, brass, ferrous alloys and many more metals. It is not suitable for aluminum and magnesium.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 - 1.36 g/cc1.27 - 1.36 g/cc
pH 0.00 - 0.600.00 - 0.60
Viscosity 6400 - 7400 cP6400 - 7400 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 105 °C221 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 95.0 - 425 °C203 - 797 °FSoldering Range
 
Descriptive Properties
FormClear Gel
Spread Factor>80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey JM1090 Soft Solder/Flux
Johnson Matthey Mattisol B Soft Solder/Flux
Johnson Matthey LM™ 195 Indium Bearing Soft Solder Alloy
Johnson Matthey JM3070 Soft Solder/Flux

NSFLUX031 / 185715

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.