MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chase Electronic Coatings HumiSeal® 1C48 UV Curable Silicone Conformal Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: HumiSeal® 1C48 is a fast moisture cure, low viscosity VOC-free silicone conformal coating which provides excellent moisture and environmental protection for printed circuit assemblies. HumiSeal® 1C48 is solvent free and can be cured at room temperature in just a few minutes. HumiSeal® 1C48 is RoHS Directive 2011/65/EU compliant.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content >= 100 %>= 100 %By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 220 - 320 cP220 - 320 cPFed-Std-141, Meth. 4287
Thickness 50.0 - 200 microns1.97 - 7.87 milRecommended coating
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D2240-95
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.44e+14 ohm-cm3.44e+14 ohm-cmASTM D257
Surface Resistance 3.00e+14 ohm3.00e+14 ohmASTM D257
Insulation Resistance 4.52e+11 ohm4.52e+11 ohmMoisture; (IPC-CC-830
 5.00e+13 ohm5.00e+13 ohmMIL-I-46058C
Dielectric Strength 18.5 kV/mm470 kV/inASTM D149
 
Processing PropertiesMetricEnglishComments
Cure Time  1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
> 40% R.H.
 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
Optimum cure
Tack-Free Time  1.50 min
@Thickness 0.100 mm,
Temperature 60.0 °C
0.0250 hour
@Thickness 0.00394 in,
Temperature 140 °F
For handling. 50% RH; Fed-Std-141, Meth. 4061
 4.02 min
@Thickness 0.200 mm,
Temperature 60.0 °C
0.0670 hour
@Thickness 0.00787 in,
Temperature 140 °F
For handling. 50% RH; Fed-Std-141, Meth. 4061
 4.98 min
@Thickness 0.100 mm,
Temperature 21.0 °C
0.0830 hour
@Thickness 0.00394 in,
Temperature 69.8 °F
For handling. 50% RH; Fed-Std-141, Meth. 4061
 7.80 min
@Thickness 0.200 mm,
Temperature 21.0 °C
0.130 hour
@Thickness 0.00787 in,
Temperature 69.8 °F
For handling. 50% RH; Fed-Std-141, Meth. 4061
Shelf Life 12.0 Month
@Temperature 23.0 °C
12.0 Month
@Temperature 73.4 °F
DOM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS923 / 239784

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.