MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Muntz metal, 60%, UNS C28000, O60 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Soft Anneal

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Cold Worked

Common Fabrication Processes: Blanking; Forming and Bending; Hot Forging and Pressing; Hot Heading and Upsetting; Shearing

Typical uses: Architectural Panels; Decoration; Door Frames; Hardware; Large Architectural Trim; Large Sheets; Sheet; Structural, Heavy Plate; Decorative Hardware; Bolts; Brazing Rod; Condenser Plates; Condenser Tube; Evaporator Tubes; Heat Exchanger Tube; Hot Forgings; Large Nuts and Bolts; Valve Stems

Applicable Specifications: Bar – ASTM B36/B36M; Plate - ASTM B36/B36M; Seamless Condenser Tube & Ferrule Stock - Condenser Tube ASME SB111, Condenser Tube ASTM B111/B111M; Seamless Tube – ASME SB135; Sheet - ASTM B36/B36M; Strip - ASTM B36/B36M; Tube – Seamless (Metric) ASTM B135/B135M, ASTM B135, FEDERAL WW-T-791

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.303 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 80
@Thickness 25.4 mm
Tensile Strength 54.0 ksi
@Thickness 25.4 mm
Tensile Strength, Yield 21.0 ksi
@Thickness 25.4 mm
0.5% Ext
Elongation at Break 50 %
@Thickness 25.4 mm
Tensile Modulus 15000 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.34Calculated
Machinability 40 %
Forgeability 90 %
Shear Strength 40.0 ksi
@Thickness 25.4 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000610 ohm-cm28% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.6 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 71.0 BTU-in/hr-ft²-°F
Melting Point 1650 - 1660 °F
Solidus 1650 °F
Liquidus 1660 °F
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1150 - 1450 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 59 - 63 %
Iron, Fe <= 0.070 %
Lead, Pb <= 0.090 %
Zinc, Zn 36.8 - 41 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC28000x2 / 292904

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.