MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Main Characteristics:
  • Good ductility
  • Good corrosion resistance
Typical Applications:
  • High volume turned parts
  • Keys

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.65 g/cc0.313 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers >= 175>= 175
Tensile Strength, Ultimate 570 - 780 MPa82700 - 113000 psi
Tensile Strength, Yield >= 55.0 MPa
@Strain 0.2 %
>= 7980 psi
@Strain 0.2 %
Elongation at Break 3.0 %3.0 %100 A
Modulus of Elasticity 130 GPa18900 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000230 ohm-cm0.0000230 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 100 °C
8.89 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.410 J/g-°C0.0980 BTU/lb-°F
Thermal Conductivity 33.0 W/m-K229 BTU-in/hr-ft²-°F
Melting Point 1020 °C1870 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 63 %63 %
Lead, Pb <= 1.0 %<= 1.0 %
Nickel, Ni 13 %13 %
Zinc, Zn <= 23 %<= 23 %
 
Descriptive Properties
ColorIvory

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NCLAL085 / 160116

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.