MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling Durostone® EP-CFK/VE-CFK Epoxy or Vinylester Composite Profile
Categories: Polymer; Thermoset; Epoxy; Vinyl Ester

Material Notes:

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 - 1.60 g/cc0.0542 - 0.0578 lb/in³ISO 1183 meth 1
Water Absorption <= 0.20 %<= 0.20 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 900 - 1500 MPa131000 - 218000 psilongitudinal; ISO 527
Modulus of Elasticity 70.0 - 110 GPa10200 - 16000 ksitransverse; ISO 178
Flexural Strength 850 - 1400 MPa123000 - 203000 psitransverse; ISO 178
Compressive Strength 120 - 420 MPa17400 - 60900 psitransverse; ISO 604

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Composites 8079 Modified Vinylester SMC
Polynt POLYCOR® VINYLESTER TOOLING GELCOAT PA
Goodfellow Polyaramid/Vinylester Composite Tube or Rod
Applied Composites 175 Vinylester SMC

PROCH9095 / 232798

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.