MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. SpectraSyn™ High Viscosity (PAO) products have high viscosity indices translate into improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ High Viscosity PAO basestocks are particularly suited for industrial oils requiring high stability under extreme operating conditions. SpectraSyn™ High Viscosity PAO products are frequently used in conjunction with lower viscosity fluids (PAO, mineral oils) as a viscosity booster to achieve a wide range of ISO VG industrial and automotive gear oils.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.853 g/cc
@Temperature 15.6 °C
ASTM D4052
Brookfield Viscosity 745000 cP
@Temperature -26.0 °C
ASTM D2983
Viscosity Measurement 170Index; ASTM D2270
Kinematic Viscosity 25100 cSt
@Temperature 0.000 °C
ASTM D445
 250000 cSt
@Temperature -20.0 °C
ASTM D445
Kinematic Viscosity at 40°C (104°F) 1240 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 100 cStASTM D445
Vapor Pressure 0.100 torr
@Temperature 200 °C
ASTM D2879
Evaporation Loss 0.30 %
@Temperature 150 °C,
Time 79200 sec
ASTM D972
 2.3 %
@Temperature 205 °C,
Time 23400 sec
ASTM D972
Surface Tension 32.5 dynes/cmASTM D1331A
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.10[mg KOH/g]; ASTM D974 (mod)
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.15ASTM D924
Dielectric Breakdown 46500 V
 
Thermal PropertiesOriginal ValueComments
Pour Point -22.0 °FASTM D5950/D97
Flash Point 541 °FCOC; ASTM D92
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4715ASTM D1218
 
Descriptive Properties
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000597 (g/cc)/°CASTM D1250
Fire Point626°FCOC, ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastics Group Polifil® GFPP-30 30% Glass-Reinforced Polypropylene
Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene
ExxonMobil SpectraSyn™ 40 Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn™ 10 Polyalphaolefin (PAO) Fluid

PEX99687 / 175923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.