MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Hostacom HBG 322D C2 NATURAL Polypropylene, 33% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Hostacom HBG 322D C2 NATURAL is a 33% glass fiber reinforced PP homopolymer (coupled). It combines excellent stiffness properties with good dimensional stability and low creep under load at elevated temperatures. The product is designed for injection molding of washing machine parts in permanent contact with hot water, steam and detergents and is available in natural color. It is not intended for medical, pharmaceutical or drinking water applications. This grade is not intended for medical, pharmaceutical, food and drinking water applications.

Availability: Asia-Pacific

Application: White Goods

Market: Electrical / Electronics

Processing Method: Injection Molding

Attribute: Detergent Resistant; High Rigidity; High Tensile Strength; Steam Resistant

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-1/A
Melt Flow 9.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 103 MPa14900 psiISO 527-1, -2
Flexural Modulus 8.00 GPa1160 ksiISO 178
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179-1/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9364 / 324299

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.