MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX8120P Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 812OP resin is a 20% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This extrudable grade has excellent chemical resistance and high heat resistance. . NORYL GTX8120P resin is anodizable, has low thermal conductivity and is an excellent candidate for extruded thermal break applications.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Moisture Absorption 1.00 %1.00 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 2.5 %2.5 %ISO 62-1
Viscosity 12 cP
@Load 10.0 kg,
Temperature 280 °C
12 cP
@Load 22.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi5 mm/min; ISO 527
Tensile Strength, Yield 125 MPa18100 psi5 mm/min; ISO 527
Elongation at Break 3.5 %3.5 %5 mm/min; ISO 527
Elongation at Yield 3.0 %3.0 %5 mm/min; ISO 527
Tensile Modulus 6.80 GPa986 ksi1 mm/min; ISO 527
Flexural Strength 175 MPa25400 psiyield, 2 mm/min; ISO 178
Flexural Modulus 5.00 GPa725 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
19.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 240 °C464 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Vicat Softening Point 235 °C455 °FRate B/120; ISO 306
 235 °C455 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 100 °C176 - 212 °FCalibrator Temperature
Melt Temperature 270 - 280 °C518 - 536 °FProfile Extrusion
Drying Temperature 110 - 120 °C230 - 248 °FProfile Extrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourProfile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82144 / 290091

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.