MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC ASAHIKLIN AK-225DH Hydrochlorofluorocarbon Solvent
Categories: Fluid; Solvent

Material Notes: AK-225DH was developed as a solvent dewatering and drying system to remove water from the surface of various parts and assemblies. AK-225DH is a mixture of AK-225 and a drying agent to give it rapid water-displacing properties. It is used in specially designed vapor degreaser with all boil sumps. The existing degreaser designed for a mixture of CFC-113 and a drying agent can be used with a few modifications.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/cc
@Temperature 25.0 °C
Liquid
Viscosity 0.60 cP
@Temperature 25.0 °C
Surface Tension 16.3 dynes/cm25°C
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 34.6 cal/gb.p.
Melting Point >= -40.0 °CPrecipitation temperature of a drying agent
Boiling Point 54.0 °C
 
Descriptive Properties
KB Value31
Ozone Depletion Potential (CFC-11 = 1.0)0.033
Relative Evaporation Rate (ether=100)90
Solubility Parameter6.9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WAGC05 / 74561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.