MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: 1 inch wide, 20 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.

Design/Construction:

  • Interleave: 1 mil Polyester
  • Rubber: Self-fusing Silicone Rubber
  • Cross-section: 1" wide rectangular

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccSilicone Property; Arlon SQA-TMS-024
Water Absorption 0.10 %Arlon SQA-TMS-016
Thickness 20.0 milRubber; Arlon SQA-TMS-012
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 46Silicone Property; ASTM D2240
Tensile Strength 1428 psiSilicone Property; ASTM D412
Elongation at Break 699 %Silicone Property; ASTM D412
Peel Strength 3.40 pliBond Strength; Arlon SQA-TMS-015
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 834 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Inert 500 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.1 °C
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARL9852 / 149005

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.