MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Medium leaded naval brass, UNS C48200
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Good hot workability for hot forging, pressing, and machining operations.

Applications: marine hardware, screw machine products, valve stems.

Available as flat products, rod, shape.

Key Words: ISO CuZn37Pb1Sn1, ISO CuZn36Sn1Pb, CEN CW712R, CEN CW714R
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.44 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 386 - 517 MPa
Tensile Strength, Yield 172 - 365 MPaDepending on temper
Elongation at Break 43 %in 381 mm.
Modulus of Elasticity 100 GPa
 100 GPa
Poissons Ratio 0.28Calculated
 0.28calculated
Machinability 50 %UNS C36000 (free-cutting brass) = 100%
 50 %UNS C36000 (free-cutting brass) = 100%
Forgeability 90 %
Shear Modulus 39.0 GPa
 39.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000663 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 116 W/m-K
Melting Point 885 - 900 °C
 885 - 900 °C
Solidus 885 °C
Liquidus 900 °C
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 650 - 760 °C
Recrystallization Temperature 360 °C
@Diameter 19.0 mm
Rod cold drawn 30%
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 59 - 62 %
Iron, Fe <= 0.10 %
Lead, Pb 0.40 - 1.0 %
Tin, Sn 0.50 - 1.0 %
Zinc, Zn 38 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High Leaded naval brass, UNS C48500
Free-Cutting Brass, UNS C36000
Forging Brass, UNS C37700
Silicon Red Brass, UNS C69400
Antimonial Naval brass, UNS C46600

MC48200b1 / 11471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.