MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Moplen EP549P Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Moplen EP549P is a fast crystallization heterophasic copolymer, suitable for injection molding applications, and contains an anti-static agent. It exhibits a high stiffness combined with a medium fluidity. Customers reported that Moplen EP549P is can be used successfully in houseware, garden furniture, cylindrical containers for detergency and crates. This grade is not intended for medical and pharmaceutical applications.

Availability: Africa-Middle East; Europe

Application: Crates; Furniture; Housewares; Opaque Containers

Market: Consumer Products; Rigid Packaging

Processing Method: Injection Molding

Attribute: Contains Antistat; Impact Copolymer; Medium Flow; Medium Stiffness; Nucleated

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 15.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 1.45 GPa210 ksiISO 527-1, -2
Charpy Impact, Notched  0.550 J/cm²
@Temperature -20.0 °C
2.62 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 0.650 J/cm²
@Temperature 0.000 °C
3.09 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9663 / 324598

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.