MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Goodfellow Cobalt/Boron/Silicon/Iron/Molybdenum/Nickel Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Cobalt Alloy

Material Notes: Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 900900kg(f)/mm²
Tensile Strength at Break >= 700 MPa>= 102000 psi
Tensile Modulus 63.0 GPa9140 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000136 ohm-cm0.000136 ohm-cm
Magnetic Coercive Force, Hc 0.010 Oe0.010 Oe
Magnetic Saturation Flux Density, Bmax 7000 Gauss7000 Gauss
Curie Temperature 365 °C689 °F
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature 520 °C968 °F
Maximum Service Temperature, Air 80.0 °C176 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 12 %12 %
Cobalt, Co 69 %69 %
Iron, Fe 4.0 %4.0 %
Molybdenum, Mo 2.0 %2.0 %
Nickel, Ni 1.0 %1.0 %
Silicon, Si 12 %12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Medium-Silicon Iron, heat-resistant gray iron
Nickel-Chromium-silicon Iron, heat-resistant gray iron
High-Silicon Iron, corrosion resistant
Goodfellow Cobalt/Silicon/Boron/Iron/Nickel Alloy
H.C. Starck Ampersint® MAP FeNi 50/50 For Soft Magnets

NGOODF130 / 16204

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.