MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AGC Fluon® ZL-521N ETFE, powder
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Description: Fluon® ETFE is a melt-processable copolymer of tetrafluoroethylene and ethylene. Fluon ETFE possesses a unique combination of desirable properties such as higher resistance to heat and chemical attack and outstanding physical toughness. It is processable by conventional extrusion, injection molding, roto-molding, roto-lining, and electrostatic coating. It is available in a variety of forms including 1/8” pellets, designated as ‘P’, and powder, designated as ‘B’.

Benefits:

  • High resistance to heat: Fluon ETFE has a continuous use temperature of 150°C.
  • Excellent chemical resistance
  • Outstanding physical toughness: Fluon ETFE has better physical properties than most other fluoropolymers.
  • Low smoke and flame characteristics: Fluon ETFE is rated 94 V-0 by Underwriters Laboratories Inc.
  • Outstanding resistance to weather and aging
  • Good dielectric properties
  • Non-stick characteristics
Applications:
  • Wire & cable (automotive, industrial, aerospace, transit, and appliance markets)
  • Film and sheets
  • Tubing and pipe
  • Electronic components
  • Electrostatic and roto-molded vessel linings
  • Valves, fittings, and pump housings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 30.0 - 50.0 micronsMolded
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 300 °C
Middle Barrel Temperature 270 - 290 °C
Front Barrel Temperature 260 - 280 °C
Nozzle Temperature 290 - 320 °C
Mold Temperature 60.0 - 120 °C
Injection Velocity 1.00 - 15.0 mm/sec
Injection Pressure 50.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials IGS3723 Insulating Glass Sealant
Zircar Zirconia ZYF-50 Zirconia Felt Insulation
Vanadium (V) Oxide, V2O5
Overview of materials for Nylon 66, Unreinforced
Mo-Sci Corporation GL 0179 Borosilicate glass frit

PAGCX023 / 191132

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.