MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber for low to high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Filler Content 20 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 93.8 MPaASTM D638
Elongation at Break 1.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 15800 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 145 MPaASTM D790
Flexural Modulus 12200 MPaASTM D790
Izod Impact, Notched 27.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 - 10000 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohmASTM D257
Static Decay 0.0020 sec(Mil-B-81705C), 12% RH, 500 kV to 50 kV
Shielding Effectiveness 30 - 80 dB
@Frequency 2.0e+7 - 1.80e+10 Hz
1/8 thickness
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 299 - 316 °C
 
Descriptive Properties
FeaturesAntistatic
 Conductive
 Electrically Conductive
 Electromagnetic Shielding (EMI)
 Radio Frequency Shielding (RFI)
 Statically Conductive
FormsPellets
Generic MaterialLCP
Generic NameLiquid Crystal Polymer (LCP)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 South America
RoHS ComplianceRoHS Compliant
UsesAerospace Applications
 Automotive Electronics
 Business Equipment
 Computer Components
 Connectors
 Electrical Housing
 Electrical/Electronic Applications
 Housings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRA A950 LCP, Unfilled
RTP Company RTP 3400-3 Liquid Crystal Polymer (LCP), Unfilled
Avient Stat-Tech™ LC-20NCF/000 V3 RD 4020 Liquid Crystal Polymer (LCP)
Avient Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS)
Celanese VECTRAN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)

PH0POL1066 / 145635

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.