MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would readily attack Type 316 stainless. This alloy exhibits superior resistance to stress-corrosion cracking in boiling 20 to 40% sulfuric acid. 20Cb-3 stainless is also stabilized to limit intergranular attack, even in the sensitized condition. Corrosion tests on annealed and sensitized material conducted in the Ferric Sulfate - 50% Sulfuric Acid Test resulted in rates of 0.002 inches per month maximum. Important advantages of 20Cb-3 stainless are its excellent mechanical properties and comparative ease of fabrication. The presence of columbium in the alloy minimizes the precipitation of carbides during welding. Assemblies usually have been placed in service in the as-welded condition.

This material has found wide use in all phases of the chemical and allied industries. It has been used extensively in the processing of synthetic rubber, high-octane gasoline, solvents, explosives, plastics, synthetic fibers, heavy chemicals, organic chemicals, pharmaceuticals, and agrichemicals. 20Cb-3 stainless has also been used in SO2 scrubbers where acid content, such as sulfuric acid, is of more concern than high-halogen content, such as chlorides. Other applications have included use in fans, mixing tanks, agitators, distillation towers, heat exchangers, process piping, bubble caps, metal cleaning and pickling tanks, spray pickling equipment, pump shafts and rods, valve stems, bolts, nuts, washers, tie rods, continuous-line pickling equipment including racks, etc.

20Cb-3® is a registered trademark of Carpenter Technology Corporation.

Key Words: ASTM B472; ASTM B473; ASTM B474; ASTM B471; ASTM B472; ASTM B473; ASTM B474; ASTM B475; ASTM B729, Carpenter Technology Corporation, Carpenter Steel Division; Cartech, UNS N08020; NACE MR0175; ASTM A265; ASTM B366; ASTM B462; ASTM B463; ASTM B464; ASTM B468; ASTM B471
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.08 g/cc0.292 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 627 MPa90900 psi
Tensile Strength, Yield 331 MPa
@Strain 0.2 %
48000 psi
@Strain 0.2 %
Elongation at Break 45 %45 %In 50 mm
Reduction of Area 67 %67 %
Tensile Modulus 193 GPa28000 ksi
Poissons Ratio 0.310.31
Fatigue Strength 330 MPa
@# of Cycles 1.00e+7
47900 psi
@# of Cycles 1.00e+7
R.R. Moore Test, Smooth Rotating Beam
Shear Modulus 73.7 GPa10700 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0001082 ohm-cm0.0001082 ohm-cm
Magnetic Permeability 1.0021.002
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.69 µm/m-°C
@Temperature 25.0 - 100 °C
8.161 µin/in-°F
@Temperature 77.0 - 212 °F
 15.91 µm/m-°C
@Temperature 25.0 - 450 °C
8.839 µin/in-°F
@Temperature 77.0 - 842 °F
 17.15 µm/m-°C
@Temperature 25.0 - 900 °C
9.528 µin/in-°F
@Temperature 77.0 - 1650 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Chromium, Cr 19 - 21 %19 - 21 %
Copper, Cu 3.0 - 4.0 %3.0 - 4.0 %
Iron, Fe 36 %36 %as remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %2.0 - 3.0 %
Nb + Ta <= 1.0 %<= 1.0 %
Nickel, Ni 32.5 - 35 %32.5 - 35 %
Niobium, Nb (Columbium, Cb) <= 1.0 %<= 1.0 %min Nb = 8 x C content
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.035 %<= 0.035 %
Tantalum, Ta <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 316L Stainless Steel, annealed plate
Carpenter 20Cb-3® Stainless Steel
AISI Type 316L Stainless Steel, annealed sheet
Carpenter 20-Mo6® Stainless Steel, Plate
420 Stainless Steel

NCAR90 / 15685

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.