MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Microtherm Group Thin Sheet Filament Reinforced Silica Thermal Insulation Sheet
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® Thin Sheet is Microtherm® Insulation manufactured in a standard thickness of 3mm although thinner versions may be available on request. It can be rolled around a cylindrical object and it is suitable for punching out small shaped profiles for applications such as thermal protection to electronic components.
    Properties
  • Formulation based on pyrogenic silica with a mineral oxide opacifier and E-glass filament reinforcement
  • Ultra thin microporous insulation
  • Can be formed by gentle rolling into curved shape
  • Capable of continuous exposure to temperatures up to 1000°C (1832°F)
  • Environmentally friendly
  • Free of harmful respirable fibers.
    Typical applications
  • Ultra thin high temperature protection
  • Heat shields for delicate electronics
  • Missile guidance systems heat shielding
  • Intelligent armaments

Information provided by Microtherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 - 0.450 g/cc0.0116 - 0.0163 lb/in³
Thickness 3000 microns118 mil
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  0.680 J/g-°C
@Temperature 0.000 °C
0.163 BTU/lb-°F
@Temperature 32.0 °F
 0.920 J/g-°C
@Temperature 200 °C
0.220 BTU/lb-°F
@Temperature 392 °F
 1.00 J/g-°C
@Temperature 400 °C
0.239 BTU/lb-°F
@Temperature 752 °F
Thermal Conductivity  0.0225 W/m-K
@Temperature 100 °C
0.156 BTU-in/hr-ft²-°F
@Temperature 212 °F
@ 320 kg/m³
 0.0233 W/m-K
@Temperature 200 °C
0.162 BTU-in/hr-ft²-°F
@Temperature 392 °F
@ 320 kg/m³
 0.0248 W/m-K
@Temperature 300 °C
0.172 BTU-in/hr-ft²-°F
@Temperature 572 °F
@ 320 kg/m³
 0.0271 W/m-K
@Temperature 400 °C
0.188 BTU-in/hr-ft²-°F
@Temperature 752 °F
@ 320 kg/m³
 0.0300 W/m-K
@Temperature 500 °C
0.208 BTU-in/hr-ft²-°F
@Temperature 932 °F
@ 320 kg/m³
Maximum Service Temperature, Air 1000 °C1830 °Ffor long term exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA), High Impact
Microtherm Group Quilted Panel Filament Reinforced Silica Thermal Insulation Panel, Flexible
Overview of materials for Acetal Copolymer, Unreinforced

CMICRO21 / 90063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.