MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Freudenberg Sealing Technologies NBR NB702717 Nitrile Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nitrile rubber exhibits superior mechanical strength with high elasticity as well as good deformation behavior. Its relatively low heat resistance can be traced to the presence of reactive double bonds. It is used for oil- and fuel-resistant seals such as Simmerrings®, O-rings and frame seals. The use of NBR marked the arrival of elastomers as a sealing material particularly in general industry.

Information provided by Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070DIN 53505
Tensile Strength 15.0 MPa2180 psiDIN 53504
Elongation at Break 340 %340 %DIN 53504
Compression Set  13 %
@Temperature 0.000 °C,
Time 259000 sec
13 %
@Temperature 32.0 °F,
Time 72.0 hour
DIN 53517, A
 13 %
@Temperature 100 °C,
Time 79200 sec
13 %
@Temperature 212 °F,
Time 22.0 hour
DIN 53517, A
 31 %
@Temperature 100 °C,
Time 605000 sec
31 %
@Temperature 212 °F,
Time 168 hour
DIN 53517, A
 44 %
@Temperature -20.0 °C,
Time 259000 sec
44 %
@Temperature -4.00 °F,
Time 72.0 hour
DIN 53517, A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °Ftest; ASTM D1329, TR10
 -30.0 °C-22.0 °F
 -23.0 °C-9.40 °Ftest; ASTM D1329, TR50
Brittleness Temperature -34.0 °C-29.2 °FDIN 53546
 
Descriptive Properties
Colorblack
Cross-linkingsulfur

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFREU9293 / 293815

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.