MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 30 µm. Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³
Thickness 30.0 microns1.18 mil
Melt Flow 0.90 g/10 min
@Load 2.16 kg
0.90 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.9 MPa1730 psi
Film Tensile Strength at Yield, TD 12.1 MPa1750 psi
Film Elongation at Break, MD 310 %310 %
Film Elongation at Break, TD 590 %590 %
Coefficient of Friction 0.200.20
Elmendorf Tear Strength MD 370 g370 g
Elmendorf Tear Strength TD 240 g240 g
Elmendorf Tear Strength, MD 12.3 g/micron312 g/mil
Elmendorf Tear Strength, TD 8.00 g/micron203 g/mil
Dart Drop 2.70 g/micron68.6 g/mil
Film Tensile Strength at Break, MD 24.1 MPa3500 psi
Film Tensile Strength at Break, TD 19.8 MPa2870 psi
 
Optical PropertiesMetricEnglishComments
Haze 4.4 %4.4 %
Gloss 75 %75 %45°
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 °C379 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow LDPE 607A Low Density Polyethylene, High Clarity Blown Film Grade
Dow LDPE 955I Low Density Polyethylene
Dow LDPE 779I Low Density Polyethylene
Dow LDPE 5004IM Low Density Polyethylene
Dow LDPE 510I Low Density Polyethylene

PDW506 / 34575

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.