MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® GA616050 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Applications
PETROTHENE GA 616-050 is a linear low density polyethylene resin which can be dry blended with low density polyethylene coating resins to produce linear low extrusion coatings. LDPE grade NA 204-000 (0.918 density, 7.0 melt index) is the preferred low density polyethylene resin for this blend.

Processing Techniques
Specific recommendations for processing GA 616-050 can only be made when the processing conditions, equipment and end use are known. The maximum recommended melt temperature for GA 616-050 blended with LDPE is 625°F. Suggested blend ratios can be obtained by contacting your Equistar sales representative.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Index of Compound 7.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56Type IV Specimen; ASTM D2240
Tensile Strength at Break 1700 psiType IV Specimen; ASTM D638
Elongation at Break 870 %Type IV Specimen; ASTM D638
Flexural Stiffness 50000 psiType IV Specimen; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 92.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene GA574200 Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene
Westlake Hifor LT74105 Linear Low Density Polyethylene

PEQU0687 / 37156

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.