MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

En-Door ED-G78 PVC External Lubricant
Categories: Other Engineering Material

Material Notes: General Information: ED-G78 is high efficient and intensified compound PVC external lubricant containing metal salts. It is well compatible with PVC resin and all kinds of stabilizers. It can improve free fluidity, stability and surface luster of products. Non-toxic. It is equivalent to related products of Henkel.

Application: ED-G78 is suitable for transparent products. It is widely used in PVC processing, such as granules, rigid sheets, compressed thin films and shrinkable films, food and medicine packaging, water supply pipes, etc. The Recommended dosage is 0.3-1.0 phr for 100 phr PVC resin.

Information provided by En-Door

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 2.0 %
@Temperature 105 °C,
Time 7200 sec
<= 2.0 %
@Temperature 221 °F,
Time 2.00 hour
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 18<= 18[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 115 °C230 - 239 °F
Flash Point >= 250 °C>= 482 °F
 
Descriptive Properties
AppearanceWhite or yellowish flake or powder
Iodine value<2gI2/100g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENDOOR039 / 316673

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.