MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture sealing. CONSIL-E is available in a variety of standard cross-sections: rectangular, round, “D” shape, “U” channels, “P” shapes and various thin wall constructions. Custom cross sections are available per customer specifications. CONSIL-E is designed to provide reliable cost effective shielding and is especially ideal for a wide range of commercial and telecommunications EMI applications

Applications: CONSIL-E is intended primarily for groove an flange mounting applications.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 - 2.35 g/cc1.85 - 2.35 g/ccASTM D792
Deformation 10 %10 %3.7 pli; 0.06" OD by 0.04" ID tube
 30 %30 %11 pli; 0.06" OD by 0.04" ID tube
 50 %50 %17.8 pli; 0.06" OD by 0.04" ID tube
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 53 - 6753 - 67ASTM D2240
Tensile Strength >= 0.345 MPa>= 50.0 psiASTM D412
Elongation at Break >= 50 %>= 50 %ASTM D412
Tear Strength 3.51 kN/m20.0 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.030 ohm-cm<= 0.030 ohm-cm
Shielding Effectiveness  65 dB
@Frequency 100000 Hz
65 dB
@Frequency 100000 Hz
H-Field
 >= 90 dB
@Frequency 1e+10 Hz
>= 90 dB
@Frequency 1e+10 Hz
Plane Wave
 >= 100 dB
@Frequency 1e+9 Hz
>= 100 dB
@Frequency 1e+9 Hz
Plane Wave
 >= 130 dB
@Frequency 1e+7 Hz
>= 130 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Descriptive Properties
BinderSilicone
ColorTan
FillerSilver-plated glass particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic

PCHOME367 / 131077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.