MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Universal Wire Works A Nickel Alloy Welding Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Alloy A is used for arc welding various dissimilar combinations of austenitic and ferritic steels and high nickel alloys. For example, when welding Inconel and Incoloy type alloys to carbon steel, stainless steel, Nickel 200, Monel type alloys, and nickel alloys, it is the product of choice. Alloy A is used to weld Monel type alloys, Nickel 200, and carbon steel to stainless steels. Alloy A is recommended for welding Incoloy type alloy 800 and 9% nickel steel to themselves. Electrode sizes 3/32 and 3/16 diameter can be used in all positions, while the larger 5/32 and 3/16 diameter are normally used in the flat or horizontal positions. POWER SUPPLY DCRP.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS A5.11 Class ENiCrFe-2; ASME SFA-5.11 Class ENiCrFe-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 552 MPa80000 psi
Elongation at Break 30 %30 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Chromium, Cr 13 - 17 %13 - 17 %
Cobalt, Co <= 0.12 %<= 0.12 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe <= 12 %<= 12 %
Manganese, Mn 1.0 - 3.5 %1.0 - 3.5 %
Nickel, Ni >= 62 %>= 62 %
Niobium, Nb (Columbium, Cb) 1.0 - 2.5 %1.0 - 2.5 %
Other <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.020 %<= 0.020 %
Tantalum, Ta <= 0.30 %<= 0.30 %
Titanium, Ti <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NUWW136 / 19654

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.