MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cast Silicon Bronze, UNS C87800, M05 Temper, As Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Permanent Mold Cast

Casting Characteristics: High – Casting Yield, Fluidity; Medium – Gassing, Effect of Section Size, Shrinkage in Solidification; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding; Good Suitability - Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Oxyacetylene Welding

Typical uses: Brackets; Clamps; Hexagonal Nuts; General Hardware; Brush Holders; Corrosion Resistant Components; Gears; High Strength, Thin Walled Die Castings; Lever Arms; Pump Impellers; Tools; Valve Parts; Marine Hardware; Plumbing Parts

Applicable Specifications: As Die Cast – Castings ASTM B176, Castings SAE J461, Castings SAE J462; As Permanent Mold Cast – Castings ASTM B806; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8181
Tensile Strength 572 MPa83000 psi
Tensile Strength, Yield 255 MPa37000 psi0.5% Ext
Elongation at Break 29 %29 %
Tensile Modulus 138 GPa20000 ksi
Machinability 40 %40 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000260 ohm-cm0.0000260 ohm-cm6.7% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.6 µm/m-°C
@Temperature 20.0 - 300 °C
10.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 2.31 W/m-K16.0 BTU-in/hr-ft²-°F
Melting Point 821 - 916 °C1510 - 1680 °F
Solidus 821 °C1510 °F
Liquidus 916 °C1680 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.15 %<= 0.15 %
Antimony, Sb <= 0.050 %<= 0.050 %
Arsenic, As <= 0.050 %<= 0.050 %
Copper, Cu >= 80 %>= 80 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb <= 0.090 %<= 0.090 %
Magnesium, Mg <= 0.010 %<= 0.010 %
Manganese, Mn <= 0.15 %<= 0.15 %
Nickel, Ni <= 0.20 %<= 0.20 %
Phosphorus, P <= 0.010 %<= 0.010 %
Silicon, Si 3.8 - 4.2 %3.8 - 4.2 %
Sulfur, S <= 0.050 %<= 0.050 %
Tin, Sn <= 0.25 %<= 0.25 %
Zinc, Zn 12 - 16 %12 - 16 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC87800x3 / 293186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.