MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cadmium-Copper, Deoxidized, UNS C14300
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: anneal resistant electrical applications requiring thermal softening and embrittlement resistance, lead frames, contacts, terminals, solder-coated and solder-fabricated parts, furnace-brazed assemblies and welded components, cable wrap.

Available as flat products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 221 - 400 MPa
Tensile Strength, Yield 76.0 - 386 MPaDepending on temper
Elongation at Break 42 %in 25.4 mm.
Modulus of Elasticity 115 GPa
Poissons Ratio 0.30Calculated
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %
Shear Modulus 44.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000179 ohm-cm96% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Thermal Conductivity 377 W/m-K
@Temperature 20.0 °C
Melting Point <= 1080 °C
Solidus 1926 °F
Liquidus 1080 °C
Annealing Point 1000 - 1400 °F
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 0.10 %
Copper, Cu 99.9 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phosphorus deoxidized arsenical Copper, UNS C14200
Cadmium-Copper, Deoxidized, UNS C14300 H08 Temper
Cadmium-Copper, Deoxidized, UNS C14300 OS025 Temper
Cadmium-Copper, Deoxidized, UNS C14310
Cadmium Copper, UNS C16200, OSO25 Temper flat products

MC14300b1 / 10608

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.