MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Monprene® CP-19141 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-19141 is a high performance thermoplastic elastomer, designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-19141 is a clear, low hardness, low density, unfilled, lubricated grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; High Flow; Low Density; Low Specific Gravity; Low Hardness; Lubricated; Slip; Without Fillers

Uses: Bushings; Consumer Applications; Flexible Grips; Gaskets; Grommets; Handles; Knobs; Luggage; Plugs; Rubber Replacement; Soft Touch Applications; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  42
@Time 5.00 sec
42
@Time 0.00139 hour
Injection Molded; ASTM D2240
 45
@Time 1.00 sec
45
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 6.81 MPa987 psi20 in/min, Flow; ASTM D412
 13.1 MPa1900 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  0.779 MPa
@Strain 100 %
113 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 1.64 MPa
@Strain 300 %
238 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 3.13 MPa
@Strain 100 %
454 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 4.77 MPa
@Strain 300 %
692 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 560 %560 %20 in/min, Across Flow; ASTM D412
 620 %620 %20 in/min, Flow; ASTM D412
Tear Strength 27.3 kN/m156 pli20 in/min, Flow; ASTM D624
 42.4 kN/m242 pli20 in/min, Across Flow; ASTM D624
Compression Set 17 %
@Temperature 22.8 °C,
Time 79200 sec
17 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 232 °C360 - 450 °F
Middle Barrel Temperature 188 - 238 °C370 - 460 °F
Front Barrel Temperature 193 - 243 °C380 - 470 °F
Nozzle Temperature 199 - 249 °C390 - 480 °F
Melt Temperature 199 - 249 °C390 - 480 °F
Mold Temperature 10.0 - 32.2 °C50.0 - 90.0 °F
Injection Pressure 1.38 - 5.52 MPa200 - 800 psi
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0806 / 237297

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.