Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properties and high temperature resistance. Information supplied by the manufacturer. Information from manufacturer data sheet. Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line. |