MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Abatron AboCast/AboCure 4-4/50-17 Casting Epoxy for Tooling
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.

Main Advantages:

  • Easy ratios
  • Longest pot life
  • Largest castings
  • Lowest exotherm

Main Drawbacks:

  • Needs heat cure and precise ratios

Processing: 100/10 ratio. Room temperature cure 24 hours and 2 hours at 100°C, optional post-cure 2 hours at 120°C and a second optional post-cure 2 hours at 150°C.

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.10 - 0.50 %0.10 - 0.50 %24-200 hours
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 90>= 90
Tensile Strength at Break 57.9 MPa8400 psi
Elongation at Break 1.0 %1.0 %
Flexural Strength 73.8 MPa10700 psi
Compressive Strength 194 MPa28200 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.586 - 0.669 W/m-K4.06 - 4.64 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 - 130 °C248 - 266 °F
 150 - 160 °C302 - 320 °FDeflection temperature after post-cure
 
Processing PropertiesMetricEnglishComments
Pot Life 300 - 480 min
@Temperature 25.0 °C
300 - 480 min
@Temperature 77.0 °F
1-2 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PABKW002 / 22043

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.