MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials MULTIFLEX™ G60 A 11 BT 13893 TPS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Thermoplastic Elastomer based Styrenic

Information provided by DuPont Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inISO 294-4, 2577
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
cm³/10min Volume Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 6.4 %6.4 %ISO 527-1/-2 or ISO 37
 >= 300 %>= 300 %ISO 527-1/-2 or ISO 37
100% Modulus 3.10 MPa
@Strain 100 %
450 psi
@Strain 100 %
Cross direction; ISO 527-1/-2 or ISO 37
300% Modulus 4.10 MPa
@Strain 300 %
595 psi
@Strain 300 %
ISO 527-1/-2 or ISO 37
Tear Strength 29.0 kN/m165 pliparallel; ISO 34-1
Compression Set 12 %
@Temperature 23.0 °C
12 %
@Temperature 73.4 °F
ISO 815
 24 %
@Temperature 70.0 °C,
Time 86400 sec
24 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 39 %
@Temperature 100 °C,
Time 86400 sec
39 %
@Temperature 212 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 °C374 °FOptimum
 180 - 200 °C356 - 392 °F
 
Descriptive Properties
CompatibilityPolyolefins
Flow length - pressure (MPa)8
Flow length (mm)680
PolymerTPS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4605c / 296035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.